Teak wood (Tectona grandis Lf.) in the form of sawdust a byproduct/waste from the furniture industry has a considerable amount and has not been utilized optimally. This study aims to determine the content of extractive teak wood (Tectona grandis Lf.). The method used is the hot water solubility. Muna's teak wood powder weighing 4,076 g soaked in distilled water as much as 100 ml glass flask, then heated in a water bath at a temperature of 100 oC for 3 hours. The content of extractive dissolved in a liquid further characterized using Py-GCMS. Results of the analysis of Py-GCMS to extract teak wood showed concentrations of some substances, such as Carbamic acid (70,70%), mono ammonium salt (CAS) Ammonium carbamate (70,70%), Acetic acid (CAS) Ethylic acid (10,52%), Acetic acid (CAS) Ethylic acid (2,35%), Acetic acid (CAS) Ethylic acid (3,26%), and Phenol (CAS) Izal (13,17%)
Real Time Impact Factor:
Pending
Author Name: Fendi, Dian Kurniaty
URL: View PDF
Keywords: GCMS; powder teak wood; pyrolysis
ISSN: 0853-4217
EISSN: 2443-3462
EOI/DOI: 10.18343/jipi.21.3.167
Add Citation
Views: 1